INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Repair welding procedure specification

Repair welding procedure specification

Repair welding procedure specification

(OP)
Dear anyone,

Please tell me where is required to qualify repair welding procedure specification in AWS D1.1

I have been looking for it but i can not see it in AWS D1.1

Thanks in advance.

RE: Repair welding procedure specification

Repair procedures are no different than original procedures.  Same criteria apply.   

RE: Repair welding procedure specification

(OP)
thks, but where is indication in AWS D1.1???

RE: Repair welding procedure specification

Unless stated otherwise, the provisions of D1.1 apply to all welding...repair or new.  Check the administrative provisions in the front of the code.  I don't have my copy with me, but there is a statement on scope of the code.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources