Molecular weights
Molecular weights
(OP)
Can some body please guide me what are the molecular weights of coal and char. The coal falls under lignite and sub-bituminous category.
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: Molecular weights
The best you can do is to calculate a pseudo melecular weight, based on composition
(c, moisture, ash (count as silica), sulfur, ....)
But what do you want to do with that?
RE: Molecular weights
If you are interested in other properties see:
RE: Molecular weights
RE: Molecular weights