INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

casting quality factor, ASME VIII-2 and ASME II-D, Table 5A

casting quality factor, ASME VIII-2 and ASME II-D, Table 5A

casting quality factor, ASME VIII-2 and ASME II-D, Table 5A

(OP)
Hi,

in ASME II part D, table 1A for casting material SA-216 WCC, note G1 requests the use of a casting quality factor according to ASME VIII-1 UG-24 to be applied.

ASME II part D, table 5A, for ASME VIII-2 application, doesn't specify the use of such a casting quality factor.

Is it related to chapter 3.8 of ASME VIII-2 which specifies that cast material shall be submited to (Radiographic or Ultrasonic) and (Magnetic Particle or Liquid Penetrant) Examination; which would imply a casting quality factor of 1?

yours truly,

tigny

 

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources