Tensile Fatigue of High Strength Bolts
Tensile Fatigue of High Strength Bolts
(OP)
Question-
Table 5.2 of RCSC lists the Maximum Tensile Fatigue Stress of A325 bolts for 500,000 cycles as 31.0 ksi.
If you work out Eqn A-3-1 of Appendix 3 of AISC 360-05 for N=500,000 and Cf=3.9x10^8 as noted in Section 3.4 then the design stress range = 9.2 ksi.
Does this mean the maximum stress cannot exceed 31.0ksi and the max range cannot be more than 9.2 ksi?
Table 5.2 of RCSC lists the Maximum Tensile Fatigue Stress of A325 bolts for 500,000 cycles as 31.0 ksi.
If you work out Eqn A-3-1 of Appendix 3 of AISC 360-05 for N=500,000 and Cf=3.9x10^8 as noted in Section 3.4 then the design stress range = 9.2 ksi.
Does this mean the maximum stress cannot exceed 31.0ksi and the max range cannot be more than 9.2 ksi?