INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Multiple procedure qualification

Multiple procedure qualification

Multiple procedure qualification

(OP)
I am part of a project that requires qualifying welding procedures to API 1104. The welders must qualify to a 12" X.250"wall inverted tee and 12" X .250" wall butt weld to multiple qualify to all procedures.  My questions are:
1. Do we need all the procedures qualified before the weld tests?
2. Do we have to retest welders to the same tests again if we add a procedure that fits under the umbrella of the test welds?

Thank you,

Mark
 

RE: Multiple procedure qualification

1.  If the test weld is not serving as a simultaneous procedure qualification and welder qualification exercise, then yes (see subclause 6.1).  

2.  Not if the essential variables of 6.3.2 are not violated.

Steve Jones
Materials & Corrosion Engineer

http://www.linkedin.com/pub/8/83b/b04
 

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources