INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Jet Fuels

Jet Fuels

Jet Fuels

(OP)
Hi,
I would like to know if Reinforced PTFE is compatible with JP-8 and JP-10 jet fuel as well as Diesel Fuel? I am trying to find a fire safe ball valve in a 1" pipe size and the seats only seem to be in R-PTFE which does not seem to be compatible with JP-8. Any suggestions?
Thanks
Gabriel

RE: Jet Fuels

(OP)
I do agree with ione, and from experience, you can't go wrong with Viton. The only situation that I had a problem with Viton was when I had low temperatures. Other than that, it's compatible with almost everything!!  

RE: Jet Fuels

What is the reinforcement, glass fiber?  Don't know why JP-8 would attack that, nor any other hydrocarbon fuel.

RE: Jet Fuels

(OP)
Thank ione, this chart shows that JP-8 & JP-10 is ok with PTFE. This is perfect.

Now I need to find which metals are OK with JP-8/JP-10. Stainless is OK for sure but my main concern is Bronze.

RE: Jet Fuels

The engine manufacturers likely have listings of approved materials for contact with the fuel.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources