RE: 24J8 Joists circa 1965
24J8 - Resisting Moment 540,000 #-in
Max End Reaction 5,000 #
Wtg per foot 12.4 lbs
At 30' span 333 #/ft from table for total load.
The info is from Standard Load Table May 30, 1961. The next one I have after that is for H-Joists 1971