Dimension problem in Abaqus?
Dimension problem in Abaqus?
(OP)
Dear all,
I am simulating a shot impact onto a circular steel plate. The shot is defined as a rigid sphere with initial velocity 75 m/s. The SI (mm) is used throughout the simulation and the following material data.
Material, name=steel
*Density
7.8e-09,
*Elastic
210000., 0.3
*Plastic
200.2, 0.
246., 0.0235
294., 0.0474
374., 0.0935
437., 0.1377
480., 0.18
When I submit the job it runs forever and never completes. Any ideas where I might have gone wrong?