INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

12Cr P-T Chart?

12Cr P-T Chart?

12Cr P-T Chart?

(OP)
Where can I find pressure-temperature ratings for 12 Chrome material (i.e., 410, 410S, 405, etc.)?  B16.5 does not include 12Cr.

RE: 12Cr P-T Chart?

sb533023, correct, it does not, therefore you won't find them.

A common approach is to evaluate the design per a recognized Code, such as Sec VIII, Div 1, Apx 2 for flanges (and hope for the best).

Regards,

Mike

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources