INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Torsional toughness tests ASTM E143

Torsional toughness tests ASTM E143

Torsional toughness tests ASTM E143

(OP)
Does anyone have any experience with these tests being conducted in lieu of traditional Charpy impact tests?

Thanks

RE: Torsional toughness tests ASTM E143

Technically, ASTM E143 is a test for shear modulus, not toughness.  I assume that someone is referencing this method for a test setup that torsionally loads a cylindrical specimen until fracture?  I have used torsion testing before, but not in lieu of charpy impact tests.  Can you provide some additional detail on the application and why a torsion test is being specified?

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources