INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Flanges from round stock?

Flanges from round stock?

Flanges from round stock?

(OP)
Our fabrication standards prohibit making flanges for valves or pipe fitting from round stock?

What is the difference between flanges from plate, or milled from stock?

What about cutting slices from round stock that arises concerns in making flanges?

RE: Flanges from round stock?

Round stock can have hidden flaws, most likely in the direction of rolling.  They would become radial-ish defects in a slice of round.

Plate can also have hidden flaws, again most likely in the direction of rolling.  They would become interlaminar gaps within a flange, parallel to the faces.  ... possibly weakening the flange a bit less than would a radial flaw.

 

Mike Halloran
Pembroke Pines, FL, USA

RE: Flanges from round stock?

Depends on the specification; ASTM reworked a few flange specs years ago,to prohibit the practice, when users had problems with flanges cut from plate. Most ASTM specs now only permit plate for blind flanges.  

RE: Flanges from round stock?

what type of flanges ASTM or API?

Petrotrim Services
www.petrotrim.com

RE: Flanges from round stock?

(OP)
Navsea (Navy Flanges)

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources