R-Value for Air Entrained Concrete
R-Value for Air Entrained Concrete
(OP)
All,
I am seeing that air entrained concrete has a higher R-Value than standard poured concrete (see below). Whereas it makes sense, the difference surprises me. Is air-entrained concrete really this good at insulating?
Standard Concrete: R = 0.8 (F*h*sqft/BTU)/in
Air Entrained Concrete: R = 3.9 (F*h*sqft/BTU)/in
If so, how much air needs to be entrained? The standard 6% +/- per volume? Is anyone aware of an actual source / experiment where this 3.9 value was determined?
MJB
I am seeing that air entrained concrete has a higher R-Value than standard poured concrete (see below). Whereas it makes sense, the difference surprises me. Is air-entrained concrete really this good at insulating?
Standard Concrete: R = 0.8 (F*h*sqft/BTU)/in
Air Entrained Concrete: R = 3.9 (F*h*sqft/BTU)/in
If so, how much air needs to be entrained? The standard 6% +/- per volume? Is anyone aware of an actual source / experiment where this 3.9 value was determined?
MJB






RE: R-Value for Air Entrained Concrete
RE: R-Value for Air Entrained Concrete