anyone know a material that meets this criteria? used on a labtop
anyone know a material that meets this criteria? used on a labtop
(OP)
Ability to be colored
High Gloss
Easy Injection
Min-Izod 11ft/lb/in
Reasonable Tensile Strength and Modulus
Minimum Tensile Strength 7525 psi
Modulus of 300 ksi
Creep modulus of 230,000 psi @1000hrs
Density of 1.11 g/cc or less
CLTE .000047 in/inf
DTUL 264 psi @212F
UL94 Flammability rating of HB
LOI=23%02
Dielectric Strength of 510 kv/in
Comparative tracking index of 300v
High Gloss
Easy Injection
Min-Izod 11ft/lb/in
Reasonable Tensile Strength and Modulus
Minimum Tensile Strength 7525 psi
Modulus of 300 ksi
Creep modulus of 230,000 psi @1000hrs
Density of 1.11 g/cc or less
CLTE .000047 in/inf
DTUL 264 psi @212F
UL94 Flammability rating of HB
LOI=23%02
Dielectric Strength of 510 kv/in
Comparative tracking index of 300v






RE: anyone know a material that meets this criteria? used on a labtop
http://www.matweb.com
You can also try RTP
http://www.rtpcompany.com/index.htm
When you narrow it down come back for experienced based comments on the subjective values. I am sure we can help so long as you fill in a few blanks about the real world requirements.
Regards
Pat
See FAQ731-376: Eng-Tips.com Forum Policies for tips on use of eng-tips by professional engineers &
http://eng-tips.com/market.cfm
for site rules
RE: anyone know a material that meets this criteria? used on a labtop
...or did you missspell "laptop" i.e. a portable computer?