INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Equivalant to SAE J1392

Equivalant to SAE J1392

Equivalant to SAE J1392

(OP)
looking for an equivalant to SAE J1392 or G40.21-44W
 

RE: Equivalant to SAE J1392

SAE J1392 is now obsolete and has been replaced by SAE J2340.  SAE J2340 uses only SI units, so 050X according to J1392 is now called 340X in J2340.  ASTM A1008 (cold rolled) and ASTM A1011 (hot rolled) also specify HSLA steels in sheet/coil form.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources