Best Vacuum heat treating furnace
Best Vacuum heat treating furnace
(OP)
Dear all,
I am looking for a Vacuum heat treating furnace to anneal Stainless steel parts.
Which are from your experience some reputable Manufacturers?
Got Solar so far...
Thanks
I am looking for a Vacuum heat treating furnace to anneal Stainless steel parts.
Which are from your experience some reputable Manufacturers?
Got Solar so far...
Thanks





RE: Best Vacuum heat treating furnace
SECO/WARWICK
http://www.secowarwick.com/vacuum.html
ALD-Holcroft
http://ww
Ipsen
http://www.ipsenusa.com/vacuum_furnaces.shtml
Surface Combustion
http://
RE: Best Vacuum heat treating furnace
Hope it helps.
RE: Best Vacuum heat treating furnace
We used Ipsen vacuum furnaces at a heat treating facility where I worked in another lifetime. I worked there as a furnace operator and later as a metallurgical process engineer.
I cannot recall having any notable problems with Ipsen.