Speicifically I am looking for yield strength for A36 or A516-60 at 1200°F. Required for some 'thermal straightening' calcs ... thanks in advance.
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
Carbon steel tensile properties at 1200¦F?
|
RE: Carbon steel tensile properties at 1200¦F?
YS *.3
Source - Mechanical Properties of Structural Steel at Elevated Temperatures and After Cooling Down
Jyri OUTINEN and Pentti MÄKELÄINEN
Laboratory of Steel Structures,
Department of Civil and Environmental Engineering,
Helsinki University of Technology
P.O. Box 2100, FIN-02015 HUT, Finland
RE: Carbon steel tensile properties at 1200¦F?
RE: Carbon steel tensile properties at 1200¦F?
http://ww