Coating on particles or microcapsules
Coating on particles or microcapsules
(OP)
Anyone have any ideas on putting a coating onto a reactive solid amine particles, or amine microcapsules?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
Coating on particles or microcapsules
|
RE: Coating on particles or microcapsules
http://w
RE: Coating on particles or microcapsules
William Gunnar
http://www.IndustrialCoatingsWorld.com
RE: Coating on particles or microcapsules
the coating has to be very impermeable to amine molecules. I'd like to put a coating to microcapsules with a reactive amine core. I'll need to embedded the amine capsules into an epoxy matrix, and then cure the matrix at elevated temperature (350F) for 3hrs. If there is no coating, the amine would diffuse into the epoxy matrix. So I need a material that is not impermeable for amine molecules, and the coating materials has to be adhere to epoxy well.
Thanks a lot,
RE: Coating on particles or microcapsules
You also need to look at silica, broad term, encapsulation for your application. I've been look for a source that rings a bell, but haven't found it yet. Epoxy likes silica and silica likes epoxy and it is inert to the amine.
http://www.rtdodge.com/dodge_Applications.html