INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Pickling/passivation stainless steel vessel/tanks UK companies

Pickling/passivation stainless steel vessel/tanks UK companies

Pickling/passivation stainless steel vessel/tanks UK companies

(OP)
Hi, Please am currently searching for any idea on the cost of pickling stainless steels vessels/tanks. please does any one have any idea how this is carried out?

NB:The vessels in questions have a dia range from 0.2 to 1.6m with the cylindrical lengths in the range of 0.7 to 9.6m.

Thanks

RE: Pickling/passivation stainless steel vessel/tanks UK companies

Talk to Anopol in Birmingham.

Their website says "In-house facilities include immersion cleaning, pickling and passivation tanks up to 35m³ capacity and 9mtrs in length although larger items can be accommodated by the use of spraying processes."

www.anopol.co.uk

RE: Pickling/passivation stainless steel vessel/tanks UK companies

(OP)
thanks. Will do.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources