Amada LC Alpha 3 laser
Amada LC Alpha 3 laser
(OP)
Could anyone tell me if amada LC Alpha 2kw machine is capable of cutting 5mm thick stainless steel clean cut with nitrogen.
We have cut this lots if times in the past but recently we are having problems.
We cut a test square cut is realy good.
We start to run the job after a few mins laser does not go throught the material.
Anyone got some cutting data or any tips ?
Thanks
We have cut this lots if times in the past but recently we are having problems.
We cut a test square cut is realy good.
We start to run the job after a few mins laser does not go throught the material.
Anyone got some cutting data or any tips ?
Thanks





RE: Amada LC Alpha 3 laser
When was the last time you had Service look at your internal/external optics?