A350 LF2 flange for ammonia transportation pipeline
A350 LF2 flange for ammonia transportation pipeline
(OP)
Hi!
Instead of A350 LF2 What material I can use? for example AISI 310 stainless steel or 316?
Thanks a lot.
Instead of A350 LF2 What material I can use? for example AISI 310 stainless steel or 316?
Thanks a lot.





RE: A350 LF2 flange for ammonia transportation pipeline
I thonk 304L and 316(L) will do the job.
RE: A350 LF2 flange for ammonia transportation pipeline
Lets forget about the stainless steel..Any other carbon steel for using in ammonia pipeline as being flange..A350 LF2 is not very easy to find and purchase for me so that I need anything else instead of it..
RE: A350 LF2 flange for ammonia transportation pipeline