Convergence Problem using Biphasic Material to model a hip joint
Convergence Problem using Biphasic Material to model a hip joint
(OP)
Dear All,
i am new to this forum and would like say hello to everybody!
I am currently working on a hip joint model consistent mainly
of the cartilogenous tissues. Biphasic Materials consitent of
a linear elastic Matrix and trapped fluid, which i modelled in
abaqus using Soil Mechanics (permeability).
At the moment, however, i am unable to obtain convergence. The
whole calculation stops at ca 0.122 sec out of total 1 sec. I
guess its just one parameter set wrong in Contact or an convergence criteria! Would be very thankful for any help.
[Material is validated against Literiture first modeled as a plug,
Elements are C3D20RP, unsymetric solver is used due to curved contact surfaces and biphasic material.]
Cheers
Felix
i am new to this forum and would like say hello to everybody!
I am currently working on a hip joint model consistent mainly
of the cartilogenous tissues. Biphasic Materials consitent of
a linear elastic Matrix and trapped fluid, which i modelled in
abaqus using Soil Mechanics (permeability).
At the moment, however, i am unable to obtain convergence. The
whole calculation stops at ca 0.122 sec out of total 1 sec. I
guess its just one parameter set wrong in Contact or an convergence criteria! Would be very thankful for any help.
[Material is validated against Literiture first modeled as a plug,
Elements are C3D20RP, unsymetric solver is used due to curved contact surfaces and biphasic material.]
Cheers
Felix