M42 bolt
M42 bolt
(OP)
Hi all,
Quick question can someone please point me in the direction of an M42 bolt table that include, UTS / Shear single and double. (grade 8.8)
thanks.
Quick question can someone please point me in the direction of an M42 bolt table that include, UTS / Shear single and double. (grade 8.8)
thanks.





RE: M42 bolt
Yield strength: 8 *0.8*1000 = 640 N/mm^2 = 640 MPa
Design strength (TENSILE)
fk,N ( 8.8) = MIN (0.7 * Tensile strength; Yield strength) = 0.7*800 = 560 N/mm^2 = 560 MPa
Design strength (SHEAR): fk,N/SQRT(2) = 396 MPa