Fillet Weld Qualification by Groove Weld Tests
Fillet Weld Qualification by Groove Weld Tests
(OP)
Hi all,
Do welders, who are qualified for Groove Welds (diameter: 0.5 inch thickness:2.77mm , position : 6G), also qualify for 3/8 inch socket welds?
Could you please clarify?
Thanks
Do welders, who are qualified for Groove Welds (diameter: 0.5 inch thickness:2.77mm , position : 6G), also qualify for 3/8 inch socket welds?
Could you please clarify?
Thanks





RE: Fillet Weld Qualification by Groove Weld Tests
RE: Fillet Weld Qualification by Groove Weld Tests
RE: Fillet Weld Qualification by Groove Weld Tests
Your sizes would normally be limited by QW=403.16 and QW-404.30, except as permitted by QW-303.1.
Table QW-452.6 might help convince you.
RE: Fillet Weld Qualification by Groove Weld Tests