INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

TQ 50 temper definition and cost

TQ 50 temper definition and cost

TQ 50 temper definition and cost

(OP)
For a housing, our manufacturer is to use the Aluminum Bronze UNS C95300.
Matweb gives this in the "as cast" and "TQ50 temper" condition, with the TQ50 temper exhibiting better properties.

2 Questions:
1: What is the process assoicated with bringing it to the TQ50 temper condition?
2: What is a rough estimate of the cost increase, in percent, associated with specifying a component in the TQ50 temper condition compared to without any quenching and tempering? We are looking at a part weighting 400 lbs.

Any input is greatly appreciated!

  

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources