Sheet Metal Thickness
Sheet Metal Thickness
(OP)
Hi,
I have a question in regards to ProE/SheetMetal (2001 version). I design all my sheet metal parts at a thickness of 1mm. After a couple days, I check the thickness again and the thickness of the parts are now down to 0.853mm. This is true for over 300 pieces... I just noticed this issue, and we have been designing sheet metal parts for over 7 years now.
Can anyone help me with this issue?
Thanks!
I have a question in regards to ProE/SheetMetal (2001 version). I design all my sheet metal parts at a thickness of 1mm. After a couple days, I check the thickness again and the thickness of the parts are now down to 0.853mm. This is true for over 300 pieces... I just noticed this issue, and we have been designing sheet metal parts for over 7 years now.
Can anyone help me with this issue?