SlipFit
SlipFit
(OP)
Hi
What is slip fit?
I searched machinery hand book, but could not find information on slip fit.
Where can find the tolerances for slip fit?
What is the standard way of designating slip fit? For example we use H7/p6 for press fit similarly what we specify for slip fit?
Thanks
What is slip fit?
I searched machinery hand book, but could not find information on slip fit.
Where can find the tolerances for slip fit?
What is the standard way of designating slip fit? For example we use H7/p6 for press fit similarly what we specify for slip fit?
Thanks





RE: SlipFit
hole shaft
basis basis
Locational clearance: H7/h6 H7/h6
Sliding H7/g6 G7/h6
Close running H8/f7 F8/h7
Free running H9/d9 D9/h9
Loose running H11/c11 C11/h11
No slip fit?
RE: SlipFit
TygerDawg
Blue Technik LLC
Virtuoso Robotics Engineering
www.bluetechnik.com
RE: SlipFit
If you are using ISO Tol. you need to get a booklet for the shop. DIN 7157 / ISO 286
RE: SlipFit
As correctly pointed out by ASimpson, there are classification of fits which are application specific. He lists the metric version, imperial are equivalents noting 1.0 inch = 25.4 mm.
There are several good references on this, look to the web. But the Machinist Handbook does discuss this, at least in the 23rd edition.
Kenneth J Hueston, PEng
Principal
Sturni-Hueston Engineering Inc
Edmonton, Alberta Canada