L-605 cracking
L-605 cracking
(OP)
What is the major cause of cracking in L-605 alloy?
We have struggled with problem on and off for years and never figured it out.
Thank you
We have struggled with problem on and off for years and never figured it out.
Thank you





RE: L-605 cracking
Can you provide some additional background information as to use of this material in service??? What type of cracking???
RE: L-605 cracking
The major amount of cracking has been of a stress corrosion type making our cleaning suspect.
However we also trying to anneal with a vacuum furnace and the ramp up to temperature is slow
and the quench is on boarder line of being to slow.
Thank you
RE: L-605 cracking
RE: L-605 cracking
We are trying to use a 2 bar vac furnace with helium argon mix