INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

WPS as AWS D1.1 require

WPS as AWS D1.1 require

WPS as AWS D1.1 require

(OP)
Dear,

i have just stared to make one WPS as AWS D1.1 but i don't know how to begin.

Please tell me step by step to carry out one WPS

RE: WPS as AWS D1.1 require

This request falls along the lines of "please tell me how to design a piping system," or "please tell me how to build a pressure vessel."  There are very similar reasons as to why a company hires welding engineers and consultants - there are an infinite number of applications, variables, design conditions, materials, etc.  

It may be wise for your company to do the same, or, should you choose to tackle this yourself, read D1.1 Section 4 "Qualification" front to back, and browse Annex N for some sample forms to get an understanding of the variables and documentation that will be involved along the way.

RE: WPS as AWS D1.1 require

duongwe,

Agree with Mr168, your best option would be to hire a consultant to do this work.

And you will probably have to read Section 4 more than once to understand it fully.

RE: WPS as AWS D1.1 require

If a "prequalified joint" WPS can be used, you had better also read Chapter 2 & 3. You might also wish to purchase an appropriate AWS Standard Welding Procedure.  

Based on your current lack of knowledge as you have stated, you're better off hiring a consultant.

RE: WPS as AWS D1.1 require

(OP)
Thanks all,
But i am a person not company so i want to be far of knowledge. today we will begin to make PWPS? how about PWPS? How to prepare best PWPS? How about check list for PWPS?
Someone could help me...
Thanks in advance!

RE: WPS as AWS D1.1 require

Your best bet is to read AWS D1.1...probably more than once as it can be confusing.   

RE: WPS as AWS D1.1 require

duongwe

While you're only a "person not a company," we're presuming that you are doing this for your company and not for a home project.  If your company has not bought a copy of AWS D1.1, then you need to tell them that you have to have it -- the whole thing. Then you need to read it, as previously suggested.

Patricia Lougheed

******

Please see FAQ731-376: Eng-Tips.com Forum Policies: Eng-Tips.com Forum Policies for tips on how to make the best use of the Eng-Tips Forums.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.