INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Shear force of disc magnets

Shear force of disc magnets

Shear force of disc magnets

(OP)
Hi,

Lets say I have two disc magnets of equal size that are stuck together with zero air gap.  Are there any analytic methods for determining the shear force required to separate the two magnets?  I've found formulas for determining the normal force required to separate the magnets, but not the shear force.  

RE: Shear force of disc magnets

No, you'll have to resort to FEA/BEA to calculate the magnetic force of attraction.  You'll have to specify the amount of displacement because the shear force will be zero if they are perfectly aligned.  

Don't forget, you'll have frictional forces to overcome too.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources