Hello to everyone!
I'm running a project wich includes a series of t-peel tests and i have to do a simulation of the t-peel test method using Ansys.
Has anyone any idea how to program this in Ansys?
Thank you in advance!
I'm running a project wich includes a series of t-peel tests and i have to do a simulation of the t-peel test method using Ansys.
Has anyone any idea how to program this in Ansys?
Thank you in advance!





RE: T-Peel Test
There are multiple cohesive element types in ANSYS that employ a traction-separation relationship to model adhesive failure. I would focus on using the INTER205 element.
Regards