we have a small project where the customer wants a welders log on a spreadsheet. Does anyone have a simple example?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: welder log
Date/Welder ID/Weld Joint number/Root/Fill
12/6/ 1234 / weld A1/ GTAW/SMAW
RE: welder log
We use weld mapping and tracking separate from our welder logs. Our welder logs are used primarily for maintaining welder continuity and to assist with HR functions. A separate log helps rod room attendants verify that the welder has the necessary qualifications to have the requested filler issued to him/her.
If you can better define what the customer is looking for, we can probably offer something a bit more insightful.
Some question to ask: is NDE involved at all? Are your welders assigned stencil numbers? Are they assigned employee ID numbers? Are they qualified on different materials with different fillers? Are field weld numbers assigned to your weld joints, or is the welding primarily structural? etc.
RE: welder log
RE: welder log