INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

RT or Shearwave? New Pipeline What codes and Laws

RT or Shearwave? New Pipeline What codes and Laws

RT or Shearwave? New Pipeline What codes and Laws

(OP)
RT or Shearwave? New Pipeline What codes and Laws are required to be legal?

Is Xray required?

Can shearwave be used in leiu of Xray?

I can't find any thing in Part 195.

And does API 1104 override Part 195?

Thanks Ken

RE: RT or Shearwave? New Pipeline What codes and Laws

195 is the law.  It references 1104.  There should be no conflicts, although if there is, 195 would normally govern, as that is the legal requirement.  What supposed conflict are you suggesting is creating the problem?

A certain amount of x-raying is required, as is stated in 195 and B31.4.  

See 195 for the law, and B31.4 for additional guidance.  Any differences there, you would normally follow 195, or if significantly different, ask either or both parties, or your boss, for clarifications.

RE: RT or Shearwave? New Pipeline What codes and Laws

DOT has approved UT in lieu of RT on numeroaus pipeline installations.

RE: RT or Shearwave? New Pipeline What codes and Laws

If you wish to replace RT by UT a written procedure and practical procedure qualification on a sample with known simulated flaws in it is essential.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources