Cracks on IP nozzle ring segment
Cracks on IP nozzle ring segment
(OP)
Helo,
we found some cracks on nozzle ring segment. We are thinking what to do next - replacement of the nozzle or repair. What are yours suggestions?
Steam properties in front the nozzle: p=39[bar] t=520[C]
we found some cracks on nozzle ring segment. We are thinking what to do next - replacement of the nozzle or repair. What are yours suggestions?
Steam properties in front the nozzle: p=39[bar] t=520[C]





RE: Cracks on IP nozzle ring segment
http:/
RE: Cracks on IP nozzle ring segment
RE: Cracks on IP nozzle ring segment
RE: Cracks on IP nozzle ring segment
RE: Cracks on IP nozzle ring segment
RE: Cracks on IP nozzle ring segment
what stage is this on?
RE: Cracks on IP nozzle ring segment
Based on your drawing, this nozzle assy looks to be a weldment. And the cracks appear to be in one of the weld zones (specifically, right where the drawing specifies "R16"). Is this correct?
Terry