ASME B16.34, paga. 6.1.6 (b)
ASME B16.34, paga. 6.1.6 (b)
(OP)
Can someone please clarify ASME B16.34, paga. 6.1.6 (b)?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
ASME B16.34, paga. 6.1.6 (b)
|
RE: ASME B16.34, paga. 6.1.6 (b)
do = the inner diameter (per the rules defined in the paragraph)
to = the minimum wall
So lets say your inner diameter is 12" and your minimum wall is 3"
3*12 = 36, sqrt(36)= 6
6*0.35 = 2.1
So if you draw a circle around the area on the casting that is under the required minimum wall section that circle must be less than or equal to 2.1" in diameter.