INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Visual Measurement System

Visual Measurement System

Visual Measurement System

(OP)
We are considering getting a Ram Optical system with their eBx software for the Q.C. dept.  Is anyone familiar with this product?  Advice...recommendations...pros and cons.  Any input would be helpful.   Thanks

    Jim Walker
 Southwest Quality Molding

RE: Visual Measurement System

I haven't used the Ram system, but we used an optical system, very rudimentary, to inspect spinnerets made in house.  We had three machines, two with what would be called an inspection microscope and one with a TV camera.
On the microscopic machine we had a XY table controlled by stepping motors with measurement and adjustments made with differential micrometers using operator input.  We used reticules along with the micrometers to measure C/L distance and circularity of the up to 1280 0.009" holes.  We had the same three point measurement for holes used by the Ram system. We had no edge measurement.  I like the Ram system where you can put in the limits of the feature.
A Ram system would have fit in our program like a glove.  

I would suggest several things. If possible get   demonstration of the system using a known particular part, or better yet a visit to distributor for a hands on demonstration.  If you get to make the visit be sure to checkout the competency of their technical people.  The factory people are usually very good though some of distributor's people leave a lot to be desired.
 

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources