INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

welding A297 HD ( GX40CrNiSi 27-4) with AISI 1020

welding A297 HD ( GX40CrNiSi 27-4) with AISI 1020

welding A297 HD ( GX40CrNiSi 27-4) with AISI 1020

(OP)
hi all
 anyone here can help me  in this problem:
i have to join by GMAW a pipe material: ASTM A297 HD  also DIN: GX40CrNiSi27-4 also UNS: J93005  with  AISI 1020 carbon steel. can anyone tell me
1)wich material use to jon them
 2 preheating temperature
  3) cooling rate?
any help is apprecite
thanks
 matteo

RE: welding A297 HD ( GX40CrNiSi 27-4) with AISI 1020

Do you work in a company? Is the first time your company does this?

RE: welding A297 HD ( GX40CrNiSi 27-4) with AISI 1020

(OP)
yes first time
 why do you ask?
 

RE: welding A297 HD ( GX40CrNiSi 27-4) with AISI 1020

If it is not the first time, I suppose there must be files in your company that can help

RE: welding A297 HD ( GX40CrNiSi 27-4) with AISI 1020

(OP)
definetly first time we have to weld those materials.
do you have info about? where are you from? i m italian
ciao

RE: welding A297 HD ( GX40CrNiSi 27-4) with AISI 1020

I am Spanish. Sorry I can not help you, never done it before-

Ana

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources