Stress Relieving UHMWPE
Stress Relieving UHMWPE
(OP)
Can anyone advise on process required to stress relieve uhmwpe sheet up to 75 mm thick, I have machined a mould for use in a microwave and it has distorted quite considerably, I would like details of the process required to anneal uhmwpe prior to machining after rough machining and after final machining. Thanks