thinning LPS3
thinning LPS3
(OP)
I have 2 old jugs of LPS3 that are much thicker than I recall. I'd like to thin the LPS3 with some solvent that will evaporate harmlessly (to the LPS3) after application.
Suggestions?
thanks
Dan T
Suggestions?
thanks
Dan T





RE: thinning LPS3
Rod
RE: thinning LPS3
CASRN
Weight Percent
Aliphatic Hydrocarbon
64742-47-8
60 - 70%
Distillates Petroleum Hydrotreated Heavy Paraffinic
64742-54-7
5 - 10%
Propylene Glycol Mono-n-butyl Ether
5131-66-8
5 - 10%
Dipropylene Glycol Mono Butyl Ether
29911-28-2
1 - 5%
Light Mineral Spirits
64742-88-7/8052-41-3
1 - 5%
You could add a little more mineral spirits