What will be the filler wire & electrode to weld A 312 TP 317L material by GTAW & SMAW process as per ASME sec IX.
also confirm the 'A' for weld metal. A quick reply is highly appreciated
also confirm the 'A' for weld metal. A quick reply is highly appreciated





RE: filler wire
SFA 5.9 ER317L GTAW
A No is 8