INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

organic acid (fatty acid) corrosion mechanism

organic acid (fatty acid) corrosion mechanism

organic acid (fatty acid) corrosion mechanism

(OP)
Hi,

we have to transport (piping) and store (storage tank)tallow at a temperature of 150F with a TAN of 6.2 mg KOH/gr, Sulphur at 50 ppmwt, Nitrogen at 236 ppmwt, Na at 53 ppmwt, Ca at 5 ppmwt, K at 40 ppmwt, P at 194 ppmwt, Mg at 11 ppmwt and Si at 17 ppmwt.  

Do you think Carbon steel will be appropriate for the service for both equipment (piping and storage tank)?

Do you have good references to suggest me on the subject to help me out in my final decision?

Thank in advance,

hcjulien

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources