What means class 2 in this indication A 350 LF 6 class 2 - class of pressure ?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: A 350 LF 6 Class 2
-TJ Orlowski
RE: A 350 LF 6 Class 2
RE: A 350 LF 6 Class 2
RE: A 350 LF 6 Class 2
RE: A 350 LF 6 Class 2
RE: A 350 LF 6 Class 2
or average of three specimens - minimum 20 ft-lbs.
RE: A 350 LF 6 Class 2
RE: A 350 LF 6 Class 2
RE: A 350 LF 6 Class 2
Read the specification! I just answered your question above.