Smart questions
Smart answers
Smart people
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Member Login

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips now!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!

Join Eng-Tips
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

LINK TO THIS FORUM!

Add Stickiness To Your Site By Linking To This Professionally Managed Technical Forum.
Just copy and paste the
code below into your site.

Partner With Us!

"Best Of Breed" Forums Add Stickiness To Your Site
Partner Button
(Download This Button Today!)

Feedback

"...I always seem to find what I need in previous threads without starting my own. I have started a couple but that's it..."

Geography

Where in the world do Eng-Tips members come from?
sssahoo (Materials)
23 Sep 10 11:14
I am a newbie in materials selection for petroleum production related project. I am having problems in selecting materials when the environment is highly conducive to pitting. Should I go for Duplex/Super Duplex/Alloy 625 or Alloy 825.

We will encounter very high CO2 and Cl-. Also, the operating temperature is around 90 C.  
jbeckhou (Mechanical)
23 Sep 10 18:02
See attached doc. Might help you out.

 

Petrotrim Services

sssahoo (Materials)
24 Sep 10 8:38
Hello Jbeckhou,

I appreciate your help. However, I am looking for "Performance" of the following steels in a specific environment (10 % CO2 (mol. fraction, 8000 mg/l Cl- ions and roughly 13000 MPa pressure):
1. Duplex Steels, 2. Super Duplex, 3. Alloy 625 and 4. Alloy 825.
I need to know the performance of the above steels when pitting and crevice corrosion are potential issues.

Best regards,
Samay
jbeckhou (Mechanical)
1 Oct 10 12:36
So you are looking for the Pren rating for the above materials?

Petrotrim Services

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!

Close Box

Join Eng-Tips® Today!

Join your peers on the Internet's largest technical engineering professional community.
It's easy to join and it's free.

Here's Why Members Love Eng-Tips Forums:

Register now while it's still free!

Already a member? Close this window and log in.

Join Us             Close