INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Equivalent EN grade

Equivalent EN grade

Equivalent EN grade

(OP)
Please suggest equivalent material grade in EN for ASTM A 479 Gr 304 & 316.

A quick reply is highly appreciated

RE: Equivalent EN grade

This would be a good place to start:

EN 10272:2007 Stainless steel bars for pressure purposes
 

RE: Equivalent EN grade

Lahaned,
316 = en 14401
304 = en 1.4301
note:
1)Chemical Analysis of EN 10088 ( General Purpose)is the same of EN 10028 ( pressure purpose)
2)Pay attention on Cr% of 304 . In the ASTM A479 Cr%> 18 while EN must be > 17,5%
3)EN 1.4401 Cr% 16,5 -18,5 while 316 Cr% = 16-18

RE: Equivalent EN grade

a) ASTM A 479 Gr.304 = ASME SA 479 Gr.304
UNS = S30400
W = 1.4301
EN Equivalent : EN 10263-5 Gr. X5CrNi 18-10

b) ASTM A 479 Gr.316 = ASME SA 479 Gr. 316
UNS = S31600
W = 1.4401 / 1.4436
EN Equivalent :
EN 10263-5 Gr. X3CrNiMo 17-13-3
En 10263-5 Gr. X5CrNiMo 17-12-2

Sincerely,

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources