INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Olefin and gum in gasoline (long term storage effect)

Olefin and gum in gasoline (long term storage effect)

Olefin and gum in gasoline (long term storage effect)

(OP)
Dear all,
I am seeking information about gasoline stability related to the existence of gum and olefin. My refinery has to deal with a condition where it has to blend a small amount of untreated delayed coker naphtha to the gasoline product. Even though we can minimize the proportion, still there are some issue related to specification that we need to ask,

1)    Once I read a publication mentioned that for long term gasoline storage – up to 6 months – the acceptable olefin content is 3 vol % maximum worldwide.  Is it correct? Is the number 3% has already included cyclo-olefin and cyclo-diolefin?  Should there be any special concern for the existence of those cyclo-olefin forms? If so, what is the maximum limitation for cyclo-olefin and cyclo-diolefin in gasoline?

2)    Is there any correlation between olefin content in a particular blend of gasoline with its induction period and/or the method to analyze the induction period? Once I heard that the induction period should be more than 1000 minute for a sample which has more than 20% olefin.

3)    Is it necessary to check again the olefin content and existent gum after oxidation stability test conducted to a gasoline sample (induction period test, such as ASTM D-525)? Once I saw a gasoline sample which has been analyzed twice for its existent gum (both washed and unwashed) and olefin content (once before stability test and once after). It was obvious that there are significant increases in both olefin content and gum after stability test. I just wondering whether one analysis each for olefin and gum before oxidation stability test are adequate and have already represented condition expected during long term storage.

Sorry for my lack of experience. This is a new case for me since this is the first time we deal with such an issue. Even my country's gasoline spec hasn't been specifically prepared for that. Any response will be highly appreciated.

Best regards.
 

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources