A671 - What Class?
A671 - What Class?
(OP)
Any help or suggestions would be greatly received.
We have a client that has specified the material of construction to be A671 (he has not defined a class). They are simple pipe spools ranging from 30" to 60" diameters.
They have to be suitable down to -50F.
I have suggested using 516 Gr.60. The problem I am having is determining what class they should be.
Are there rules for determining this?
I would like to go with Class 10, no HT, RT or hydro.
Thanks in advance.
We have a client that has specified the material of construction to be A671 (he has not defined a class). They are simple pipe spools ranging from 30" to 60" diameters.
They have to be suitable down to -50F.
I have suggested using 516 Gr.60. The problem I am having is determining what class they should be.
Are there rules for determining this?
I would like to go with Class 10, no HT, RT or hydro.
Thanks in advance.