M6 A2-70 bolts (ISO 3506) are tack (spot) welded using a 1x2mm fillet weld 6mm long onto a 316 SS plate to prevent rotation during bolt up. Is there a concern regarding the degradation of mechanical properties of the bolt for a service life of 30 years?
Any suggestions or further reading will be appreciated.
Kind Regards,
Richard
M6 A2-70 bolts (ISO 3506) are tack (spot) welded using a 1x2mm fillet weld 6mm long onto a 316 SS plate to prevent rotation during bolt up. Is there a concern regarding the degradation of mechanical properties of the bolt for a service life of 30 years?
Any suggestions or further reading will be appreciated.
Kind Regards,
Richard





RE: Welding of A2-70 Bolts
RE: Welding of A2-70 Bolts
M6
I'll get back on that one
And this one too...
Yes, I'm concerned about chromium depletion in the heat affected zone