6" SS Clamp Ferrule material selection
6" SS Clamp Ferrule material selection
(OP)
Dear All,
habitually we fabricate Clamp Ferrule using Rod Bar SA-479-316 for 4" dia. and less, UG-14(b)does not accept this material for 6" dia.
I think to use piping material: SA-312-TP316 , So I can machine 6" pipe Sch80 to obtain 6" ferrule.
IS IT CORRECT TO USE THIS MATERIAL. IF NO WHAT MATERIAL CAN I USE.
THANKS VERY MUCH.
LAURENT.
habitually we fabricate Clamp Ferrule using Rod Bar SA-479-316 for 4" dia. and less, UG-14(b)does not accept this material for 6" dia.
I think to use piping material: SA-312-TP316 , So I can machine 6" pipe Sch80 to obtain 6" ferrule.
IS IT CORRECT TO USE THIS MATERIAL. IF NO WHAT MATERIAL CAN I USE.
THANKS VERY MUCH.
LAURENT.