INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

thermoformed carbon fiber

thermoformed carbon fiber

thermoformed carbon fiber

(OP)
Does anyone know of a thermoformable carbon fiber laminate with a thermoplastic resin. We do not need an HDT above 200F. The carbon should be real thin and the plastic should be clear. This is for an automotive accesory. So apperance is more important than performance.

thanks,

RE: thermoformed carbon fiber

contact  MAS  epoxies- super  web site and very knowledgeable  techs.

RE: thermoformed carbon fiber

American Matrix make thermoplastic/carbon fiber laminates using nylon and continious woven carbon fiber.  Very attractive and works well in automotive applications.  

URL: www.americanmatrixcorp.com

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources