ASME section VIII specifies acceptance criterion for cold differential test pressure of relief valve which is +/- 2.5%. Can this be applied to an API valve? or API has their own set of specifications on this.





RE: set pressure allowance for API safety relief valves
You may want to have a look at API 527.
Hope this helps!
My focus: Alloy Valves Super Duplex Valves Monel Valves Incoloy Valves Titanium Valves Hastelloy Valves