INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Difference between a medical grade plastic and pharmaceutical grade pl

Difference between a medical grade plastic and pharmaceutical grade pl

Difference between a medical grade plastic and pharmaceutical grade pl

(OP)
Please,
I would readly appreciate if someone can tell me the difference between a medical grade plastic and pharmaceutical grade plastic.

I am trying to following the USP standards

RE: Difference between a medical grade plastic and pharmaceutical grade pl

I'm on the pharmaceutical side, and the goal with our plastics is chemical inertness (doesn't leach anything into drug) and low particle generation. My guess would be medical grade plastic focuses on biological inertness.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources